Stainless steel

17-4 PH
1.4542
AISI 630
Cond. H 1025

17-4PH is a precipitation-hardened martensitic stainless steel, used for pieces which require high mechanical strength, important resilience and also good fatigue resistance. This metal is remelted by using the ESR method in order to combine a good homogeneity and structural isotropy with excellent mechanical properties (longitudinal and transversal direction).

Avantages

  • Excellent mechanical properties

  • Very resilient

  • Multipurpose alloy

PDF
Plus d'info sur
17-4 PH
1.4542
AISI 630
Cond. H 1025
Contactez nous + 33 (0)4 72 14 55 00

Normes

  • ASTM A564

  • ASTM F899

  • EN 10088-3

  • NFS94-090

Formes disponibles

Diameter
  • 5 mm to 110 mm
Length
  • 3000 mm to round

En stock

Granulometry
  • Any kind of granulometry suitable to your machine

En stock

Thickness
  • On demand
Dimensions
  • On demand

Sur demande

Diameter
  • On demand
Thickness
  • On demand

Sur demande

Diameter
  • On demand
Thickness
  • On demand

Sur demande

Normes

  • AMS 5643

  • ASTM A564

Formes disponibles

Diameter
  • 25 to 200 mm
Length
  • 3600 to 4000 mm

En stock

Normes

  • AMS 5643

  • ASTM A564

Formes disponibles

Diameter
  • 25 to 200 mm
Length
  • 3600 to 4000 mm

En stock

Composition chimique

Reference standard : ASTM F899
C
  • 0% min
  • 0,06% max
Mn
  • 0% min
  • 0,7% max
Si
  • 0% min
  • 0,7% max
P
  • 0% min
  • 0,025% max
S
  • 0% min
  • 0,015% max
Cr
  • 15% min
  • 17% max
Ni
  • 305% min
  • 5% max
Nb
  • 5xC% min
  • 0,45% max
Cu
  • 3% min
  • 4,5% max
Mo
  • 0% min
  • 0,5% max
Fe
  • Balance
Haut de page

Caractéristiques mécaniques

Rm (Mpa)
≥ 1 070
Rp 0,2 (Mpa)
≥ 1 000
Density (g/cm3)
7.8
A (%)
≥ 12